My pool company did repair (raising i did not ask for, which is totally separate issue) and I am concerned about how it was done and potential of cold joint cracking and letting water outside of the shell. Anyone can share their thoughts about it? Should I be worried or not? I assume the same material (yellowish in the picture) used under coping/tile through the whole perimeter (skimmer is now lower than it needs to be too).