I talked to the Pebble tec guy today and he said we should wait 30 days to heat the pool to give it time to cure and fully dry underneath otherwise we could damage the plaster. I read on the pebble tec website you should wait 14 days. So which is accurate?
The first pool I built 10 years ago I am pretty confident we heated it right away and it was pebble tec and 10 years later our plaster was still in good condition. I do not mind waiting a couple weeks but was hoping to use the spa around Christmas time. Any input is appreciated!